In general, if the ribs are not good, it is due to the shrinkage of the material in many cases.
You can initially increase the material flow to compensate for this, or at least part of it. Increase the extrusion multiplier in 2% increments to compensate for shrinkage as closely as possible, without the flat surfaces becoming rough (too much flow in this case).